C70600 Cupronickel (90% Cu, 10% Ni, 1.4% Fe) is the standard material for seawater cooling systems in naval vessels, offshore platforms, desalination plants, and power station condensers. It combines excellent corrosion resistance in flowing...

C70600 Cupronickel (90% Cu, 10% Ni, 1.4% Fe) ist der standard material für seawater cooling systems in naval vessels, offshore platforms, desalination plants, und power station condensers. Es combines excellent corrosion widerstand in flowing seawater mit inherent biofouling widerstand — marine organisms tun nicht readily attach zu sein surface.

Quick Facts

KategorieCopper Alloy
NormASTM B466
Density8.94 g/cm³
Yield Strength105 MPa
Tensile Strength275 MPa

Global Equivalents & Cross-Reference

Alternative Standard / GradeAction
CuNi10Fe1Mn Compare
EN CW352H Compare
JIS C7060 Compare

Verwandt Materials

🧮 Material Weight Calculator

Calculate the weight based on this material's density: 8.94 g/cm³

Teilen dies seite Teilen ein X

Frequently Asked Questions

Warum ist iron added zu 90/10 cupronickel?

Der 1.4% iron addition dramatically improves widerstand zu impingement attack in hoch-velocity seawater (>2.5 m/s flow). Ohne der iron addition, der protective oxide film breaks ab und localized erosion-corrosion occurs. Dies war ein major innovation in der 1950s das enabled cupronickel's widespread adoption in naval systems.

References & International Standards

  • ASTM International. Norm Specifications für Stahl & Metal Alloys. astm.org
  • International Organization für Standardization (ISO). Metallic Materials — Cross-Referenz Database. iso.org
  • American Iron und Stahl Institute (AISI). Stahl Güte Designations & Equivalents. steel.org
  • European Committee für Standardization (CEN). EN Stahl Standards & Numbering System. cencenelec.eu