EN 25CrMo4 (1.7218): European Cr-Mo Quenched & Tempered Steel

ASTM/EN Standard · Published: 2026-06-01 · Updated: 2026-06-02

Quick Reference

A heat-treatable alloy steel grade designed for high-strength mechanical applications. Proper heat treatment is essential to achieve the specified mechanical properties.

A heat-treatable alloy steel grade designed for high-strength mechanical applications. Proper heat treatment is essential to achieve the specified mechanical properties.

Quick Facts

CategoryAlloy Steel
StandardASTM/EN Standard
Density7.85 g/cm³
Yield Strength550 MPa (80 ksi) Q&T
Tensile Strength750 MPa (109 ksi) Q&T

Global Equivalents & Cross-Reference

Alternative Standard / GradeAction
AISI 4130 Compare
DIN 1.7218 Compare
SCM420 Compare
30CrMo Compare

Related Materials

🧮 Material Weight Calculator

Calculate the weight based on this material's density: 7.85 g/cm³

Frequently Asked Questions

What heat treatment is required?

Austenitize, quench, and temper according to the material standard. The specific austenitizing temperature, quench medium, and tempering temperature depend on the desired final properties and section size.

References & International Standards

  • ASTM International. Standard Specifications for Steel & Metal Alloys. astm.org
  • International Organization for Standardization (ISO). Metallic Materials — Cross-Reference Database. iso.org
  • American Iron and Steel Institute (AISI). Steel Grade Designations & Equivalents. steel.org
  • European Committee for Standardization (CEN). EN Steel Standards & Numbering System. cencenelec.eu